Study on the Preparation of Fluoroacrylate Copolymer
Meng Xiang · Leather and Chemicals · 1999
The prepared fluorinated acrylic monomer (1/3 of the total) and solvent are put into a 4_mouth flask and raised to 70-75℃. The rest fluorinated acrylic monomer is mixed with butyl acrylate, butyl methylacrylate and propanediol ether, and added by azobisisobutyronitrile. After dissolution the mixture is added slowly into the 4_mouth flask and reacted for 4h, under the keeping temperature to obtain the title product.